Now heat the solder preform until it melts onto the center conductor. Then heat the ends of the termination sleeve for a water tight seal. Material: Transparent Modified Polyolefin, Glue Ring, Solder Ring. Operating Temperature: -55°C-125°C. Fully Recovered Temp: 130xad°C. Temp of Solder Starting Melt: 125°C. Temp of Full Solder Melt: 150°C.